All raw materials are imported from Japan SUS314, heat-resistant 1250 ℃, strong anti-oxidation and anti-carburizing.

Stainless steel mesh with those spraying methods?

Release time:

2022-04-07


Stainless SteelMesh beltthere are those spraying method?

For the pretreatment of the stainless steel mesh belt, in order to make the film adhesion strong and not easy to fall off, the surface of the stainless steel mesh belt must be pretreated before spraying. Coatings are divided into physical monotone and chemical monotone according to their own properties. The pretreatment of the Great Wall mesh belt is very interlocking, and spraying also requires a process. It is divided into three processes. The predecessors were pretreated, then sprayed, and finally monotonous.
  
The order of the three processes cannot be communicated. There are more than ten kinds of coatings, such as oil coating, natural resin, epoxy resin, phenolic resin, etc., which can be selected according to the actual situation. Monotonous stainless steel mesh belt. In order to make the coating excellent, strong and wear-resistant, it must be used after complete monotony. Different stainless steel mesh belt pretreatment method is different. Spraying methods include manual, automatic, electrostatic, electrophoresis and other methods, which can be selected according to the batch and shape of the Great Wall mesh belt.
  
Spraying depends on the type, function and curing conditions of the coating, and the spraying process and method are also different. Users can choose according to the shape, size and batch of stainless steel mesh belt. In practice, it is fast and monotonous. Solvent-volatile coatings or heat-curable coatings are usually selected. Interest is obtained after a naturally monotonous or frugal drying process. For degreasing, derusting and phosphating of steel parts, water lotion is commonly used to remove dirt and oil, and mechanical or chemical methods are used to remove rust. Phosphating is to immerse the parts in acid diluent (density 1~1.1,pH = 1~3), and the interface between the two will react.